Journal: Journal of hazardous materials

Article Title: Lead recovery and high silica glass powder synthesis from waste CRT funnel glasses through carbon thermal reduction enhanced glass phase separation process.

PMID/MRN: 27745960

Publication Date: 2017-Jan-15

Abstract:

In this study, a novel process for the removal of toxic lead from the CRT funnel glass and synchronous preparation of high silica glass powder was developed by a carbon-thermal reduction enhanced glass phase separation process. CRT funnel glass was remelted with B 2 O 3 in reducing atmosphere. In the thermal process, a part of PbO contained in the funnel glass was reduced into metallic Pb and detached from the glass phase. The rest of PbO and other metal oxides (including Na 2 O, K 2 O, Al 2 O 3, BaO and CaO) were mainly concentrated in the boric oxide phase. The metallic Pb phase and boric oxide phase were completely leached out by 5mol/L HNO 3 . The lead removal rate was 99.80% and high silica glass powder (SiO 2 purity >95wt%) was obtained by setting the temperature, B 2 O 3 added amount and holding time at 1000ĄC, 20% and 30mins, respectively. The prepared high silicate glass powders can be used as catalyst carrier, semipermeable membranes, adsorbents or be remelted into high silicate glass as an ideal substitute for quartz glass. Thus this study proposed an eco-friendly and economical process for recycling Pb-rich electronic glass waste. Copyright © 2016 Elsevier B.V. All rights reserved.